Search found 2 matches

by Frank99
Wed Feb 14, 2018 3:35 am
Forum: Boat-Building Tips & Techniques
Topic: Fast curing glue and Floorboards
Replies: 6
Views: 10723

Re: Fast curing glue and Floorboards

Thanks for the Welcome and the very useful advice! The shop is always at a minimum 60 F and 45-50% RH, so I think no problems with chalk temperature or moistness. Cove up or bead up: in the book Canoecraft it's cove up, in the Youtube Ted Moores Workshop series it's bead up, reason being that after ...
by Frank99
Tue Feb 13, 2018 8:57 am
Forum: Boat-Building Tips & Techniques
Topic: Fast curing glue and Floorboards
Replies: 6
Views: 10723

Fast curing glue and Floorboards

Hi, new here, I just ordered a Ted Moores and Steve Killing designed Prospector kit from local Dutch supplier. It will be my first strip planked canoe. I have some experience in building two 30' traditional Dutch boats (boeier) in lapstrake and carvel. But that was some 30 years ago. Ever since I've...